TERAS PQ FERRIT

TERAS PQ FERRIT

 

MODEL

G.W

SAIZ(mm)

A

Bmin

C

D

E

F

Gmin

PQ20/16

15

20.5±0.4

18.0±0.4

8.8±0.2

14.0±0.4

5.2±0.2

8.1±0.1

12.0

PQ20/20

17

20.5±0.4

18.0±0.4

8.8±0.2

14.0±0.4

7.2±0.2

10.1±0.1

12.0

PQ26/20

34

26.5±0.5

22.5±0.45

12.0±0.2

19.0±0.45

5.7±0.2

10.1±0.1

15.5

PQ26/25

40

26.5±0.5

22.5±0.45

12.0±0.2

19.0±0.45

8.0±0.2

12.4±0.2

15.5

PQ27/20

34.6

27.3±0.5

22.5min

12.0±0.2

19.0±0.45

5.8±0.25

10.1±0.25

16.0

PQ27/25

41

27.3±0.5

22.5min

12.0±0.2

19.0±0.45

8.2±0.25

12.5±0.25

16.0

PQ27.5A/20

35.6

27.5±0.5

22.3min

12.0±0.2

19.0±0.45

5.8±0.25

10.1±0.25

16.0

PQ27.5A/25

41.6

27.5±0.5

22.3min

12.0±0.2

19.0±0.45

8.2±0.25

12.5±0.2

16.0

PQ27.5B/20

34.6

27.5±0.5

22.8min

12.0±0.2

19.0±0.45

5.8±0.25

10.1±0.25

16.0

PQ27.5B/25

40.6

27.5±0.5

22.8min

12.0±0.2

19.0±0.45

8.2±0.25

12.5±0.2

16.0

PQ32/20

45

32.0±0.6

27.5±0.5

13.4±0.3

22.0±0.5

5.8±0.25

10.1±0.25

19.0

PQ32/25

52

32.0±0.6

27.5±0.5

13.4±0.3

22.0±0.5

8.3±0.25

12.5±0.25

19.0

PQ32/30

62

32.0±0.6

27.5±0.5

13.4±0.3

22.0±0.5

10.7±0.25

15.0±0.25

19.0

PQ32/35

67

32.0±0.6

27.5±0.5

13.4±0.3

22.0±0.5

12.6±0.3

16.9±0.25

19.0

PQ32.5/20

46

32.5±0.6

28.0±0.5

13.4±0.3

22.0±0.5

5.8±0.25

10.1±0.25

19.5

PQ32.5/25

53

32.5±0.6

28.0±0.5

13.4±0.3

22.0±0.5

8.3±0.25

12.5±0.25

19.5

PQ32.5/30

63

32.5±0.6

28.0±0.5

13.4±0.3

22.0±0.5

10.7±0.25

15.0±0.25

19.5

PQ33/30

61.6

33.0±0.6

28.5±0.5

13.4±0.3

22.0±0.5

10.7±0.25

15.0±0.25

20.0

PQ35/35

77.6

35.1±0.7

32.0±0.5

14.4±0.3

26.0±0.5

12.5±0.25

17.5±0.25

23.5

PQ40/40

101

40.5±0.9

37.0±0.6

14.9±0.3

28.0±0.6

14.7±0.25

19.9±0.25

28.0

PQ50/50

216

50.0±0.9

44.0±0.7

20.0±0.3

32.0±0.6

18.0±0.25

25.0±0.25

31.5

PQM27/20

31

26.8±0.4

23.0MIN

11.8±0.2

18.9±0.3

6.1±0.25

9.5±0.25

17.0

PQM27/25

37.2

26.8±0.4

23.0MIN

11.8±0.2

18.9±0.3

9.1±0.25

12.5±0.25

17.0

PQM32/20

44

32.0±0.5

28.0MIN

13.6±0.2

22.0±0.3

6.5±0.25

10.0±0.25

20.8

PQM32/25

56

32.0±0.5

28.0MIN

13.6±0.2

22.0±0.3

8.8±0.25

12.3±0.25

20.8

PQM32/30

61

32.0±0.5

28.0MIN

13.6±0.2

22.0±0.3

11.2±0.25

14.7±0.25

20.8

PQM38

32.8

38.0±0.8

32.0min

14.2±0.3

21.2±0.5

3.5±0.3

6.5±0.3

26.7

CQ28/20

56

28.0±0.4

24.6±0.4

13.25±0.25

28.0±0.4

6.7±0.25

10.2±0.25

7.6

 

MODEL

PARAMETER

AL±25%(nH/N^2)

N.W(g)

C1mm-1

Lemm

Aemm2

Vemm3

ZP40

PQ20/16

0.605

37.4

62.0

2310

3300

13

PQ20/20

0.738

45.4

62.0

2790

3100

15

PQ26/20

0.391

46.3

119.0

5490

6100

31

CPQ26/25

0.472

55.5

118.0

6530

5200

36

PQ27/20

0.411

47.6

117.0

5490

6100

31

PQ27/25

0.481

56.8

116.0

6530

5200

36.5

PQ27.5A/20

0.409

48.5

118.0

5720

6100

32

PQ27.5A/25

0.491

57.6

117.0

6750

5200

37.5

PQ27.5B/20

0.414

48.5

117.0

5670

6100

31

PQ27.5B/25

0.496

57.6

116.0

6680

5200

36.5

PQ32/20

0.326

55.5

161.0

9420

6000

42

PQ32/25

0.376

60.6

161.0

9760

5500

48

PQ32/30

0.464

78.2

161.0

12600

5150

55

PQ32/35

0.546

85.2

161.0

13300

3950

66

PQ32.5/20

0.326

55.5

161.0

9420

6000

42

PQ32.5/25

0.376

60.6

161.0

9760

5500

48

PQ32/30

0.464

78.2

161.0

12600

5150

55

PQ33/30

0.471

79.8

161.0

12850

5000

55.8

PQ35/35

0.448

87.9

196.0

17300

4860

73

PQ40/40

0.508

102

201.0

20500

4300

95

PQ50/50

0.346

113

328.0

37200

6720

195

PQM27/20

0.43

45.6

105.0

4800

5000

28

PQM27/25

0.545

57.4

105.0

6050

4800

32.5

PQM32/20

0.392

55.9

145.7

7990

5500

40

PQM32/25

0.45

65.9

145.7

9596

5000

50.5

PQM32/30

0.562

76.7

145.7

11200

4500

55

PQM38

0.378

43.6

118.0

5140.0

5800

30

CQ28/20

0.312

46.56

149.2

6948.0

7000

48.5

 

Cool tags: teras pq ferit, teras pq ferit China pengeluar, pembekal, kilang

Hantar pertanyaan

(0/10)

clearall